Improve your Quality

Indentation test (Buchholz hardness) according to DIN EN ISO 2815

The film hardness of a single-layer or multi-layer coating structure can be determined by the Buchholz indentation test. Here, an indenter is placed shock-free on the horizontally aligned surface of the organic coating to be tested and lifted off after a load period of 30 seconds. The length of the lenticular impression in the coating is measured and the indentation resistance according to Buchholz is calculated.

Area of competence

Testing standards

  • DIN EN ISO 2815

Your contacts

Wiebke Schmid

Dipl. Engineer (FH)
Head of Laboratory
Tel +49 7171 10407-51
Fax +49 7171 10407-50
Mobil +49 151 46136991

Mail schmidifo-gmbhde